Nickelvac 901 Nickel Superalloy, UNS N09901; AMS 5660, 5661
Código de producto : NI-S1507-CU-CU
Nickelvac 901 Nickel Superalloy, UNS N09901; AMS 5660, 5661, is available in Bar (Round bar, Flat bar), Ribbon, Wire, Rods, Tube, Pipe, Foil, Plate, Sheet, Strip and Forging Stock.
Contáctenos si necesita servicios personalizados. Le informaremos el precio y la disponibilidad en 24 horas.
Packing of
Standard Packing:
Typical bulk packaging includes palletized plastic 5 gallon/25 kg. pails, fiber and steel drums to 1 ton super sacks in full container (FCL) or truck load (T/L) quantities. Research and sample quantities and hygroscopic, oxidizing or other air sensitive materials may be packaged under argon or vacuum. Solutions are packaged in polypropylene, plastic or glass jars up to palletized 3130 gallon liquid totes Special package is available on request.