Inicio > Productos > Metal & Alloys > Nickel Metal And Alloys > 718Plus Nickel Superalloy,UNS N07818,Allvac 718Plus alloy (UNS N07818)

718Plus Nickel Superalloy,UNS N07818,Allvac 718Plus alloy (UNS N07818)

Código de producto : NI-S1502-CU-CU

718Plus Nickel Superalloy,UNS N07818,Allvac 718Plus alloy (UNS N07818), is available in Bar (Round bar, Flat bar), Ribbon, Wire, Rods, Tube, Pipe, Foil, Plate, Sheet, Strip and Forging Stock.

Contáctenos si necesita servicios personalizados. Le informaremos el precio y la disponibilidad en 24 horas.

Producto Código de producto Pureza Tamaño Contáctenos
718Plus Nickel Superalloy,UNS N07818,Allvac 718Plus alloy (UNS N07818)NI-S1502-CU-CUCustomizedCustomized
Packing of Standard Packing: Typical bulk packaging includes palletized plastic 5 gallon/25 kg. pails, fiber and steel drums to 1 ton super sacks in full container (FCL) or truck load (T/L) quantities. Research and sample quantities and hygroscopic, oxidizing or other air sensitive materials may be packaged under argon or vacuum. Solutions are packaged in polypropylene, plastic or glass jars up to palletized 3125 gallon liquid totes Special package is available on request.